1100 O Aluminium Plate, Bar, Tube, Coil, Foil — GB/T 3880 · ASTM B209

1100 is 99.0% pure aluminium with a controlled copper addition. That small addition lifts strength and machinability above 1050 while keeping conductivity high and formability excellent, which is why it is the default for spun, drawn and rolled parts that also get trimmed or punched. Supplied from 0.3 mm to 100 mm, in O, H14, H24 and H18.

Aluminium plate & sheetAluminium bar & rodAluminium tube & pipeAluminium coilAluminium foil

1100 — Nameplates and signage
Application reference · 1100 O · 1 / 4

Main applications

Where this grade is used in series production, as listed in our alloy data sheet.

  • Nameplates and signage
  • Deep-drawn holloware
  • Heat exchangers
  • Packaging containers

Specifications

Values per mill test certificate; tolerances to the standard named on this page unless agreed otherwise.

Alloy1100
Series1xxx
TemperO
StandardGB/T 3190 / GB/T 3880 / ASTM B209 / EN 485-2 / GB/T 6892
Thickness0.2 – 4.0 mm
Widthup to 2,650 mm
Lengthcoil ID 508 mm · 2 – 8 t
SurfaceMill finish · Coated · Slit to width
Density2.71 g/cm³
Melting range643 – 657 °C

Other tempers on request

Melting range is the typical solidus–liquidus interval for the grade.

Chemical composition

Typical limits to ASTM / EN for the alloys we roll and extrude.

Element%
Al99.00 min
Si+Fe0.95 max
Cu0.05 – 0.20
Mn0.05 max
Zn0.10 max

Mechanical properties

Typical values at room temperature for the temper shown.

PropertyValue
Tensile strength Rm90 MPa
Yield strength Rp0.235 MPa
Elongation A35 %
Hardness28 HBW

How it compares

The two alloys buyers most often shortlist against this one.

Property110010503003
Tensile strength Rm90 MPa80 MPa150 MPa
Yield strength Rp0.235 MPa35 MPa145 MPa
Elongation A35 %35 %8 %
Hardness28 HBW25 HBW40 HBW
Density2.71 g/cm³2.71 g/cm³2.73 g/cm³

1050 is purer and slightly more conductive; 1100 is stronger and machines better. If the part is punched or turned after forming, 1100 usually wins. 3003 is the stronger, more corrosion-resistant option, but it anodises less brightly. Keep 1100 where surface appearance matters.

Process and quality control

Each heat is spectro-checked and the coil is slit to the ordered width in-house. Surface is inspected under raking light for roll marks and inclusions, and thickness is logged every 20 metres.

Packing

Export packing

Certification and reports

Mill test certificate per heat, dimensional inspection report, and SGS or BV third-party inspection on request. Certificates travel with the shipping documents.