ZORLANGALUMINUM

1050 O Aluminium Plate, Bar, Tube, Coil, Foil — GB/T 3880 · ASTM B209

1050 is commercially pure aluminium: 99.5% minimum, no alloying additions, and the highest conductivity of any grade we roll. It is the grade to specify when the job needs formability, conductivity or a bright anodised finish rather than strength. We roll it from 0.3 mm sheet to 120 mm plate, in O, H14, H24 and H18, with thickness and flatness checked on-line.

Aluminium plate & sheetAluminium bar & rodAluminium tube & pipeAluminium coilAluminium foil

1050 — Foil
Application reference · 1050 O · 1 / 5

Main applications

Where this grade is used in series production, as listed in our alloy data sheet.

  • Foil
  • Conductive busbars
  • Heat sink fins
  • Nameplates and signage
  • Chemical equipment linings

Specifications

Values per mill test certificate; tolerances to the standard named on this page unless agreed otherwise.

Alloy1050
Series1xxx
TemperO
StandardGB/T 3190 / GB/T 3880 / ASTM B209 / EN 485-2 / GB/T 6892
Thickness0.2 – 4.0 mm
Widthup to 2,650 mm
Lengthcoil ID 508 mm · 2 – 8 t
SurfaceMill finish · Coated · Slit to width
Density2.71 g/cm³
Melting range646 – 657 °C

Other tempers on request

Melting range is the typical solidus–liquidus interval for the grade.

Chemical composition

Typical limits to ASTM / EN for the alloys we roll and extrude.

Element%
Al99.50 min
Si+Fe0.40 max
Cu0.05 max
Mn0.05 max
Mg0.05 max
Zn0.05 max

Mechanical properties

Typical values at room temperature for the temper shown.

PropertyValue
Tensile strength Rm80 MPa
Yield strength Rp0.235 MPa
Elongation A35 %
Hardness25 HBW

How it compares

The two alloys buyers most often shortlist against this one.

Property105011003003
Tensile strength Rm80 MPa90 MPa150 MPa
Yield strength Rp0.235 MPa35 MPa145 MPa
Elongation A35 %35 %8 %
Hardness25 HBW28 HBW40 HBW
Density2.71 g/cm³2.71 g/cm³2.73 g/cm³

1100 adds a small copper addition for slightly higher strength and better machinability, at the cost of a little conductivity. Choose 1100 when the part is formed and machined; stay with 1050 for conductors. 3003 roughly doubles the yield strength of 1050 through manganese and still welds cleanly. Move to 3003 as soon as the part has to carry load, not just shape.

Process and quality control

Composition is verified by optical emission spectrometry on every heat. Conductivity is measured on strip, and flatness is checked on a granite table before the sheet is cut to length. Mill test certificate, dimensional report and, on request, SGS inspection are issued against the heat number.

Packing

Export packing

Certification and reports

Mill test certificate per heat, dimensional inspection report, and SGS or BV third-party inspection on request. Certificates travel with the shipping documents.

Download spec sheet (PDF)

PDF, 1 page, generated from the data on this page.