ZORLANGALUMINUM

2017 T4 Aluminium Plate, Bar, Tube — GB/T 3880 · ASTM B209

2017 is the classic rivet alloy: 425 MPa tensile in T4 with 22% elongation, enough ductility to head a rivet cold and enough strength to carry shear in airframe structures. It machines and forms well, and it sits below the 460 MPa threshold in China's dual-use export list, so normal supply needs no 1C202 licence. Plate, bar and tube from stock.

Aluminium plate & sheetAluminium bar & rodAluminium tube & pipe

2017 — Aircraft and structural rivets
Application reference · 2017 T4 · 1 / 3

Main applications

Where this grade is used in series production, as listed in our alloy data sheet.

  • Aircraft and structural rivets
  • Bolts and clamps
  • General load-bearing structures
  • Repair stock

Specifications

Values per mill test certificate; tolerances to the standard named on this page unless agreed otherwise.

Alloy2017
Series2xxx
TemperT4
StandardGB/T 3190 / GB/T 3880 / ASTM B209 / EN 485-2 / GB/T 6892
ThicknessØ 6 – 300 mm
Width60 – 600 mm
Length3,000 – 6,000 mm
SurfaceMill finish · Turned · Anodised
Density2.79 g/cm³
Melting range510 – 640 °C

Other tempers on request

Melting range is the typical solidus–liquidus interval for the grade.

Chemical composition

Typical limits to ASTM / EN for the alloys we roll and extrude.

Element%
Cu3.5 – 4.5
Mg0.40 – 1.00
Mn0.40 – 1.00
Si0.80 max
Fe0.70 max
Alremainder

Mechanical properties

Typical values at room temperature for the temper shown.

PropertyValue
Tensile strength Rm425 MPa
Yield strength Rp0.2275 MPa
Elongation A22 %
Hardness105 HBW

How it compares

The two alloys buyers most often shortlist against this one.

Property201760612011
Tensile strength Rm425 MPa310 MPa380 MPa
Yield strength Rp0.2275 MPa275 MPa295 MPa
Elongation A22 %12 %15 %
Hardness105 HBW95 HBW110 HBW
Density2.79 g/cm³2.70 g/cm³2.83 g/cm³

Process and quality control

Typical properties are verified heat by heat: spectrometric composition on every melt, tensile and yield on every cast, hardness and dimensional checks before packing. A mill test certificate, dimensional report and third-party inspection (SGS or BV) are issued against the heat number.

Packing

Export packing

Certification and reports

Mill test certificate per heat, dimensional inspection report, and SGS or BV third-party inspection on request. Certificates travel with the shipping documents.

Download spec sheet (PDF)

PDF, 1 page, generated from the data on this page.

All grades