6063 T5 Aluminium Plate, Bar, Tube, Profile — GB/T 3880 · ASTM B209
6063 is the extrusion alloy: lower strength than 6061 but far better surface finish after anodising, which is why window systems, curtain wall, heat sinks and machine guarding are all made from it. We extrude from 0.3 kg/m to 30 kg/m, hold tolerance to EN 755-9, and finish in-house with anodising or powder coating.
Aluminium plate & sheetAluminium bar & rodAluminium tube & pipeAluminium profile
Specifications
Values per mill test certificate; tolerances to the standard named on this page unless agreed otherwise.
| Alloy | 6063 |
|---|---|
| Series | 6xxx |
| Temper | T5 |
| Standard | GB/T 3190 / GB/T 3880 / ASTM B209 / EN 485-2 / GB/T 6892 |
| Thickness | 0.8 – 20 mm wall |
| Width | up to 400 mm section |
| Length | up to 12,000 mm |
| Surface | Mill finish · Anodised · Powder coated |
| Density | 2.70 g/cm³ |
| Melting range | 585 – 655 °C |
Other tempers on request
Melting range is the typical solidus–liquidus interval for the grade.
Chemical composition
Typical limits to ASTM / EN for the alloys we roll and extrude.
| Element | % |
|---|---|
| Mg | 0.45 – 0.90 |
| Si | 0.20 – 0.60 |
| Fe | 0.35 max |
| Cu | 0.10 max |
| Al | remainder |
Mechanical properties
Typical values at room temperature for the temper shown.
| Property | Value |
|---|---|
| Tensile strength Rm | 175 MPa |
| Yield strength Rp0.2 | 130 MPa |
| Elongation A | 12 % |
| Hardness | 60 HBW |
How it compares
The two alloys buyers most often shortlist against this one.
| Property | 6063 | 6005A | 6061 |
|---|---|---|---|
| Tensile strength Rm | 175 MPa | 290 MPa | 310 MPa |
| Yield strength Rp0.2 | 130 MPa | 240 MPa | 275 MPa |
| Elongation A | 12 % | 10 % | 12 % |
| Hardness | 60 HBW | 90 HBW | 95 HBW |
| Density | 2.70 g/cm³ | 2.70 g/cm³ | 2.70 g/cm³ |
6005A is a little stronger than 6063 and common in European curtain wall. Where EN 755-2 calls for 6005A, we can quote it; 6063 remains the faster, cheaper route for standard sections. 6061 is 30–40% stronger and machines better, but extrudes into simpler shapes and anodises less evenly. For a loaded machined part choose 6061; for a visible profile choose 6063.
Process and quality control
Profile dimensions are checked against the drawing before finishing, and anodic film thickness is measured on every rack. Coating adhesion is tested by impact and bend, with colour measured against the approved sample.
Packing
Certification and reports
Mill test certificate per heat, dimensional inspection report, and SGS or BV third-party inspection on request. Certificates travel with the shipping documents.