6005A T6 Aluminium Plate, Bar, Tube, Profile — GB/T 3880 · ASTM B209
6005A is the rail profile alloy: 290 MPa tensile and 240 MPa yield in T6, with manganese and chromium holding strength across the weld zone so a friction-stir-welded car body keeps its section properties. Extruded to your drawing up to a 400 mm section, anodised or painted.
Aluminium plate & sheetAluminium bar & rodAluminium tube & pipeAluminium profile
Specifications
Values per mill test certificate; tolerances to the standard named on this page unless agreed otherwise.
| Alloy | 6005A |
|---|---|
| Series | 6xxx |
| Temper | T6 |
| Standard | GB/T 3190 / GB/T 3880 / ASTM B209 / EN 485-2 / GB/T 6892 |
| Thickness | 0.8 – 20 mm wall |
| Width | up to 400 mm section |
| Length | up to 12,000 mm |
| Surface | Mill finish · Anodised · Powder coated |
| Density | 2.70 g/cm³ |
| Melting range | 585 – 655 °C |
Other tempers on request
Melting range is the typical solidus–liquidus interval for the grade.
Chemical composition
Typical limits to ASTM / EN for the alloys we roll and extrude.
| Element | % |
|---|---|
| Mg | 0.40 – 0.70 |
| Si | 0.50 – 0.90 |
| Mn | 0.50 max |
| Cr | 0.30 max |
| Al | remainder |
Mechanical properties
Typical values at room temperature for the temper shown.
| Property | Value |
|---|---|
| Tensile strength Rm | 290 MPa |
| Yield strength Rp0.2 | 240 MPa |
| Elongation A | 10 % |
| Hardness | 90 HBW |
How it compares
The two alloys buyers most often shortlist against this one.
| Property | 6005A | 6063 | 6082 |
|---|---|---|---|
| Tensile strength Rm | 290 MPa | 175 MPa | 310 MPa |
| Yield strength Rp0.2 | 240 MPa | 130 MPa | 260 MPa |
| Elongation A | 10 % | 12 % | 10 % |
| Hardness | 90 HBW | 60 HBW | 95 HBW |
| Density | 2.70 g/cm³ | 2.70 g/cm³ | 2.70 g/cm³ |
Process and quality control
Typical properties are verified heat by heat: spectrometric composition on every melt, tensile and yield on every cast, hardness and dimensional checks before packing. A mill test certificate, dimensional report and third-party inspection (SGS or BV) are issued against the heat number.
Packing
Certification and reports
Mill test certificate per heat, dimensional inspection report, and SGS or BV third-party inspection on request. Certificates travel with the shipping documents.
PDF, 1 page, generated from the data on this page.