ZORLANGALUMINUM

5083 H116 Aluminium Plate, Bar, Tube, Profile — GB/T 3880 · ASTM B209

5083 is the alloy specified for welded marine structures: 4.0–4.9% magnesium gives 275–350 MPa tensile and the best seawater resistance of any common grade. In H116 or H321 temper it resists intergranular attack after welding, which is why classification societies accept it for hulls, decks and tanks. We supply plate from 3 mm to 200 mm with ultrasonic inspection on request.

Aluminium plate & sheetAluminium bar & rodAluminium tube & pipeAluminium profile

5083 — Hulls and decks
Application reference · 5083 H116 · 1 / 3

Main applications

Where this grade is used in series production, as listed in our alloy data sheet.

  • Hulls and decks
  • LNG and cryogenic tanks
  • Rail vehicle bodies

Specifications

Values per mill test certificate; tolerances to the standard named on this page unless agreed otherwise.

Alloy5083
Series5xxx
TemperH116 · H321
StandardGB/T 3190 / GB/T 3880 / ASTM B209 / EN 485-2 / GB/T 6892
Thickness0.2 – 150 mm
Widthup to 2,650 mm
Lengthup to 12,000 mm
SurfaceMill finish · PVC coated · Anodised
Density2.66 g/cm³
Melting range574 – 638 °C

Other tempers on request

Melting range is the typical solidus–liquidus interval for the grade.

Chemical composition

Typical limits to ASTM / EN for the alloys we roll and extrude.

Element%
Mg4.0 – 4.9
Mn0.40 – 1.00
Cr0.05 – 0.25
Fe0.40 max
Alremainder

Mechanical properties

Typical values at room temperature for the temper shown.

PropertyValue
Tensile strength Rm305 MPa
Yield strength Rp0.2215 MPa
Elongation A16 %
Hardness70 HBW

How it compares

The two alloys buyers most often shortlist against this one.

Property508350525A06
Tensile strength Rm305 MPa230 MPa320 MPa
Yield strength Rp0.2215 MPa195 MPa160 MPa
Elongation A16 %12 %20 %
Hardness70 HBW60 HBW70 HBW
Density2.66 g/cm³2.68 g/cm³2.64 g/cm³

5052 is cheaper, easier to form and sufficient for most sheet-metal parts; 5083 is the choice once the structure is welded and loaded, or class-approved.

Process and quality control

Every plate is ultrasonically inspected for internal defects on request, and H116 material is tested to ASTM G67 for intergranular corrosion. Tensile tests are taken transverse to the rolling direction.

Packing

Export packing

Certification and reports

Mill test certificate per heat, dimensional inspection report, and SGS or BV third-party inspection on request. Certificates travel with the shipping documents.

Download spec sheet (PDF)

PDF, 1 page, generated from the data on this page.

All grades